It is Lab Metal which is basically an aluminum air dry epoxy. No mixing or added catalyst.

It will conduct electricity, you can plate it and fill pits in parts you want to powder coat.

It is about the consistency of tooth paste and hardens quickly.

Sands and files easily. In the can you have to keep it covered with their solvent or else it will harden.