Re: M&H Flat head

Posted by Jack Vines On 2012/1/27 17:01:54
Quote:
Does the aluminum head I hear mentioned make any difference or was this an aniwarp issue?

Aluminum was used because it transfers heat more readily and allows higher compression without overheating or pinging.

Because of the evil galvanic corrosion, it's very difficult to find a sound aluminum head. Clean and check prior to paing big bucks for anything.

jack vines